porcelain shino (fwd)

updated mon 9 nov 98

 

David Orser on sun 8 nov 98



---------- Forwarded message ----------
Date: Fri, 6 Nov 1998 16:12:32 -0500 (EST)
From: David Orser
To: nudefigure@aol.com
Subject: porcelain shino

got this one from frank martin via kansas city art inst.

porcelain shino c/ 10

nephsy 39.39
spodumene 30.30
ball 17.17
soda ash 8.08
epk 5.05