search  current discussion  categories  materials - misc 

new question - egyptian paste

updated mon 24 aug 98

 

Gary Huddleston on sun 23 aug 98

------------------


I have been looking for a formula for egyptian paste that does not have an
extreamly high
soda ash content. Formulating and testing have proven excellent colors and
glaze like finishes
but the chemical body of the paste eats through and sticks to supporting =
clay
body mold.