Cameron Harman on sun 22 nov 98

John,

The pressure cooker has, in fact, been used in a number of
commercial laboratories as a substitute for an autoclave. The idea
is that steam, under pressure, will accelerate the moisture
expansion process.

Good thinking, John !

Cameron

--
**********************************************************