search  current discussion  categories  materials - kiln wash 

kiln wash flakes off

updated thu 17 dec 98

 

pam easley on wed 16 dec 98

I, too, have had a he** of a time with my newly cleaned./scraped
shelves. The new wash flakes, dries, dunts off, same as Kate's in
earlier post. HELP!!