Hi! Just thought I'd pass this along. Last night I loaded my kiln and
had space for one more pot. I had a bisqued one that wasn't glazed and
didn't have wax resist. I use Aftosa wax resist, which I love, but it
really does take a while to dry, so I grabbed the tube of Avon's
"Silicon Glove," a heavy duty hand cream, applied it to the bottom of
the pot, waited five minutes and glazed the piece - it worked
wonderfully!

Jonathan in DC