Karen Shapiro on thu 5 nov 98

Hi all,

I downloaded raku glaze recipes from "gafergus@micron.net" and find a couple
ingredients I am not familiar with (and neither is he!). Anyone know what
"G-200" and "K-200" are?
Thanks,
Karen

douglas gray on fri 6 nov 98

Karen,

Both G200 and K200 are types of potash feldspar. You could use Custer Feldspar
as a straight substitution in these recipies.

doug

In message Karen Shapiro writes:
> ----------------------------Original message----------------------------
> Hi all,
>
> I downloaded raku glaze recipes from "gafergus@micron.net" and find a couple
> ingredients I am not familiar with (and neither is he!). Anyone know what
> "G-200" and "K-200" are?
> Thanks,


============================================================================ =)
Douglas E. Gray, Assistant Professor of Art
P.O. Box 100547
Department of Fine Arts and Mass Communication
Francis Marion University
Florence, South Carolina 29501-0547

dgray@fmarion.edu
843/661-1535