Marvin S. Flowerman on sat 19 dec 98

There have been a number of messages on the subject of an Emerald Green Glaze,
^4/5/6starting with a message of Dec. 8th from Larry Phillips.
For information purposes I tried this glaze at cone 7; it turns very dark
green, almost black, matte and unattractive. That was surprising but
indicates a delicate glaze anywhere above cone 6.
If any of you who have used this glaze care to comment I would be grateful.

Marvin Flowerman (marvpots@aol.com)