search  current discussion  categories  glazes - cone 4-7 

cone 6 leather glaze-trying again!

updated sat 19 sep 98


Leslie St.Clair on fri 18 sep 98

Okay everybody I'm trying to post this glaze again. Drat these computers!
This is called "Leather" a c6cream/white buttery matt. The amount of each
ingredient will precede it. 21 dolomite. 10 gerstly borate. 9 spodumene.5
wollastonite. 27 Custer feldspar. 12 nepheline syenite.16 kaolin. Thanks