Marley Wolhud on fri 24 jul 98

Mike, am so glad you asked this! I am having the exact same problem in
my new automtic skutt 818 with the environvent! I have done two test
fires, the last with a 10 minute hold and the middle cone was barely
bent. I fired at medium though, not slow. I don't have any answers, I
thought you would like to know you aren't alone in experiencing this!