Craig Martell on mon 13 jul 98

Hi:

In my post yesterday about Gerstley Borate, I incorrectly said that GB and
wood ash will cause glazes to flocculate. The opposite is true, they both
cause deflocculation so I just want to correct that in case some of you are
wondering about this reversal of terms.

'scuuze me, Craig Martell-struggling with the facts in Oregon

Tony Hansen on tue 14 jul 98

> In my post yesterday about Gerstley Borate, I incorrectly said that GB and
> wood ash will cause glazes to flocculate. The opposite is true, they both
> cause deflocculation.

When I have used Gerstley I always had flocculation problems with it.
Same thing with wood ash, I've had flocculation with it.

--
T o n y H a n s e n thansen@digitalfire.com
Don't fight the dragon alone http://digitalfire.com