Another thing about the bubbles it happens with only the clear glaze. We
use other Amaco LG glazes on the same pieces, (3 different kinds of clay)
and no bubbles. thanks for all your suggestions! I'll report back after we
try different things that you all have offered as solutions.
Janet
New Bern, NC

Theresa L. Jones on tue 7 jul 98


Janet, please keep me posted on what you learn. If you don't mind, I would
like your email address so we can communicate on this outside of Clayart.
Sounds like Helen might also want to be in on our conversations. It's so
nice to know I am not alone with this problem. We can start a bubbling low
fire clear glaze emotional support group.

> ----------------------------Original message----------------------------
> Another thing about the bubbles it happens with only the clear glaze. We
> use other Amaco LG glazes on the same pieces, (3 different kinds of clay)
> and no bubbles. thanks for all your suggestions! I'll report back after we
> try different things that you all have offered as solutions.
> Janet