search  current discussion  categories  kilns & firing - cones & controllers 

controller unqunderied

updated thu 2 jul 98

 

Mo Cain on wed 1 jul 98

A word of thanks to all you folks who so kindly put me straight re
controllers. I received 16 responses. 14 were unequivocably in favor of
controllers without kiln sitters or timers while 2 of the folks thought
that perhaps a timer might be useful. Tomorrow we enter into the Brave
New World ( not Huxley's !!) of delayed starts, segmented ramp ups ,
holds and segmented rampdowns. Just like a kid at christmas.

Ta very much....mocain expat Brit watching England versus Argentina this
afternoon a la Coupe du Monde... this being of course the REAL football.