search  current discussion  categories  glazes - misc 

seiving glazes

updated sun 28 jun 98

 

John Baymore on mon 22 jun 98

------------------
(clip)
My least favorite thing is probably sieving glazes. I saved a bunch of
messages awhile back about the pros and cons of sieving. I should
review those. It always takes a lot longer than I expect and I usually
have some kind of kink somewhere the next day or two from all that
repetitive motion.
(snip)

For seiving glazes I can't recommend the Talisman Glaze Seive highly
enough. It will save you HOURS AND HOURS of tedious, repetitive stress
producing labor in a short period of time. Well worth the price. Been
using one for oh....maybe...... 19 years or so.

Easy to use, easy to clean, simple design (mine has never had a problem).

My only complaint is that now they make them from plastic rather than the
all aluminum one that I have. Too bad.......... feels =22cheaper=22, and =
looks
.....well.....plastic =3Cg=3E.

BEst,

...........................john

John Baymore
River Bend Pottery
22 Riverbend Way
Wilton, NH 03086 USA

603-654-2752
JBaymore=40Compuserve.com

Marley Wolhud on sat 27 jun 98

John Baymore, I tried emailing you directly, and it didn't work. What
size mesh do you recommend for theTalisman Sieves?

Thank you