Jennifer M. Dubats on wed 10 jun 98

Marcia,

Your weathered bronze glaze was posted as:

Lithium Carb 2
Strontium 40
Neph Syn. 120
Flint 18
Ball clay 20

Add Titanium 5
Copper Carb 5

I gave this glaze to a friend and they questioned the amount of Nepheline
Syenite.
Is this correct?