k 200 feldspar?

updated sun 31 may 98

 

Rafael Molina-Rodriguez (Rafael Molina-Rodriguez) on fri 29 may 98

Clayarters :

Is K 200 a potash or soda feldspar? TIA.

Rafael

Dennis Davis on sat 30 may 98

Rafael Molina-Rodriguez (Rafael Molina-Rodriguez) wrote:

> ----------------------------Original message----------------------------
> Clayarters :
>
> Is K 200 a potash or soda feldspar? TIA.
>
> Rafael

K-200 and G-200 both are potash feldspars. An analysis from Hamill &
Gillespie (vintage unknown but at least 10 years old) for K-200 is:

67.10 SiO2
18.30 Al2O3
.07 Fe2O3
.36 CaO
Trace MgO
10.10 K2O
3.80 Na2O

LOI .18

Dennis in Stafford, VA

Grimmer on sat 30 may 98

Rafael Molina-Rodriguez (Rafael Molina-Rodriguez) wrote:
>
> ----------------------------Original message----------------------------
> Clayarters :
>
> Is K 200 a potash or soda feldspar? TIA.
>
> Rafael

Potash. It's got just about the highest K content of any spar.
Super for blue, blue, celadons. A current (or any) analysis
escapes me.
steve grimmer