search  current discussion  categories  glazes - misc 

lavender glaze?

updated fri 22 may 98

 

Ioway1 on thu 21 may 98

Hope this is not too general of question...I am responsible for keeping the
glazes up at the fine arts studio, where I volunteer, and have been trying to
replace the Cone 10 Lavender glaze . for the Gas kiln firings,....no one knows
where the recipe is, so I thought I would come up with another...The results
we are used to have a nice pale lavender color, and layer well over other
glazes and are still definable....
..Can anyone suggest a recipe I might use? I mix 10 to 20 gallons at at time.
It might be time for a change to a new recipe anyway,,, thanks in advance

Patricia Joslin Smith
Black Bear Pottery
http://members.aol.com/Ioway1/pubpage.htm
e-mail Ioway1@aol.com