Talbott on fri 24 apr 98

Jan..
I know nothing about the "Critter"... Also dipping is still our
primary method of glaze application. We also pour and use a slip trailer
and do some spraying. For larger items we use a large RubberMaid 10 gal
container to dip these bigger items into. Spraying is relatively slow and
leaves a different texture to the glaze. I don't think spraying is
essential as a method of glaze application but it does have its place for
certain affects... Marshall