search  current discussion  categories  materials - copper 

best conditions to fire for copper reds...

updated sat 11 apr 98

 

Talbott on fri 10 apr 98

Coincidence??? The best copper red firing we ever had was on a hot and
humid day during the summer.. coincidence or not?? Perhaps the still air
reduced volitization of the copper, and the low air density made for better
reduction conditions... Marshall

http://www.PotteryInfo.com

101 CLAYART MUGS (Summer 1998)
2ND ANNUAL CLAYARTERS' GALLERY - NAPLES, MAINE (Summer 1998)
E-MAIL ME FOR APPLICATIONS

Celia & Marshall Talbott, Pottery By Celia, Route 114, P O Box 4116,
Naples, Maine 04055-4116,(207)693-6100 voice and fax,(call first)
---------------------------------------------------------------------