I use the Lee's Incredible Kiln Wash from Axner Pottery Supply Co..
It almost never flakes for me at least. We used to lose a lot of nice
pottery due to kiln wash flakes with other kiln wash products and that was
unacceptable. We fire ^10 reduction in a gas kiln and we use Nitride
Bonded SiC shelves from New Castle Refractories Co. Because of the hard
nature of the shelves we are able to use the Lee's. I like having a wash
on the shelves as it make glaze drip clean-ups far easier. So for our
situation the Lee's fits our needs. I still only apply the Lee's to one
side of our shelves.
....Marshall

http://www.PotteryInfo.com

101 CLAYART MUGS (Summer 1998)
2ND ANNUAL CLAYARTERS' GALLERY - NAPLES, MAINE (Summer 1998)
E-MAIL ME FOR APPLICATIONS
http://fmc.utm.edu/~dmcbeth/cag/naples.htm

Celia & Marshall Talbott, Pottery By Celia, Route 114, P O Box 4116,
Naples, Maine 04055-4116,(207)693-6100 voice and fax,(call first)
Clayarters' Live Chat Room, Fri & Sat Nites at 10 PM EDT & Sun at 1 PM EDT
http://webchat12.wbs.net/webchat3.so?Room=PRIVATE_Clayarters

---------------------------------------------------------------------