KarenzPotz on thu 5 mar 98

Hi
I'm looking for a cone 10 black slip recipe that holds a true black even
when hit with soda. The few recipes I've tried all bleach out to a blue when
hit with the soda and most of the recipes I've found have cobalt in them and I
believe they'll do the same thing. Any suggestions please let me know this
problem drives me nuts!!


Thanks
Karen...........

Mmpottery on fri 6 mar 98

I have tried black underglaze and it holds a true black.( in salt/soda) Cover
Coats from Mile High Ceramics but others have them too. Michelle