>to anyone in clayart,
>I was wondering if there was a diference when I bisque to cone 06 or cone
>08

Yes Cone 08 is not as hot, the bisque works will be softer & absorb more
glaze.
Some gasses may not burn out at the lower temps you might see more pin holes
or even body bloating.