for the glaze guru's in the group:

I use the following red glaze cone 10 reduction, only it has some fit =
problems
for my clay body.

RED Cone 10

CUSTER 752.675
COLEMANITE 103
WHITING 112.5
TIN OXIDE 9.675
ADD
COPPER CARB. 4.5

It seems very short, as in it needs some flint. I have adjusted the formula=
as
follows:

RED REVISED Cone 10

CUSTER 752.675
COLEMANITE 103
WHITING 112.5
TIN OXIDE 9.675
FLINT 176

ADD
COPPER CARB. 4.5

will this help??? all in put is greatly welcomed.