search  current discussion  categories  glazes - cone 4-7 

raspberry glaze-cone 5 --to the creator

updated fri 27 feb 98


Sue Hintz on thu 26 feb 98

About a month or two ago someone shared a glaze called Raspberry using
mason stain 6006. I've been testing it and loving it AND having some
problems with it and wanted to learn more from the developer. In particular
I have had some crazying and if I get it on the thick side it leaves pin holes.

But I'm more concerned about the crazing. By the way, this base looks nice
over slips. I cut off the part of the e-mail that included the person
who contributed it and would love to have the chance to talk with you. Thanky
you for sharing it. This glaze has the potential of changing things for me