search  current discussion  categories  forms - sculpture 

(no subject)salt sculpture clay body

updated fri 20 feb 98

 

Ann Zerger, Associate AIA and Chip Parker, AIA on thu 19 feb 98

Hello clay artists,

Any one out there have a great sculpture clay body, that works well in
salt, I do alot of large scale architectural pieces, sometimes the body
I use will crack, particuraly when used in a plaster mold. It is a
formula I have from Don Ritz, 50 AP Green, 50epk Kaolin, 10 custer
spar, 15 flint, and 12 silica sand. Thanks Anny
email c1pwd@midusa.net