JFTRT on tue 17 feb 98

Carol Ratliff & others-

I have used the Periwinkle glaze for 5 years on several clay bodies, and it seem
be one of the most agreeable glazes of my lot.
Up here in Alaska we use Seattle Pottery Supply and they state "When subbed for
add 15-25% more Ultrox". I have done none of that "subbin" in my use of the gla
It works best over a dark red/brown clay body. Good luck!

Todd Turek