Is anyone using or have you used autumn yellow cone 10R?? If so how
much reduction does it require?? How matt is this glaze?? I fire light
reduction to neutral in a gas kiln. Currently I'm using a spodumene
glaze but it's just coming out too dry for me. I'm looking for a more
buttery feel. I tested Ferguson's yellow but it seemed to require more
reduction than I use.

Thanks for any help!!!
Gene Arnold
mudduck@triad.rr.com

William & Susan Schran User on sun 26 aug 12


On 8/26/12 2:49 PM, "Gene Arnold" wrote:

>Is anyone using or have you used autumn yellow cone 10R?? If so how
>much reduction does it require?? How matt is this glaze?? I fire light
>reduction to neutral in a gas kiln. Currently I'm using a spodumene
>glaze but it's just coming out too dry for me. I'm looking for a more
>buttery feel. I tested Ferguson's yellow but it seemed to require more
>reduction than I use.

Gene - We used this glaze when we fired to cone 10 at school.
Light reduction, fast firing, about 8 hours to cone 10.
Nice smooth mat to semi mat depending on application thickness and clay
body.
The glaze is listed on my website with image.

Bill
--
William "Bill" Schran