Thanks for the responses regarding the smelly, moldy glaze. I called
Georgie's today and was told that there is an organic compound in the glaze
that sometimes will go off. They recommended I put a few drops of bleach in
and that I may need to do it a few times to take care of it. I think I'll
add bleach and then screen it, then add a few more drops once screened so
it gets the smallest particles. Hopefully that'll take care of it!