search  current discussion  categories  kilns & firing - wood 

wood firing opportunity near washington dc

updated fri 8 jun 12

 

Sailoor47@AOL.COM on thu 7 jun 12


=3D20
Hi All,=3D20
I am doing my wood firing events a bit differently this year. =3D20
I am cutting down on the size of each group in order to give more hands on=
=3D
=3D20
help and guidance (if needed) and also to cut down on dead time for=3D20
participants in larger groups.=3D20
The old cost was $225 for 1/8 of the Manibigama II. The new cost is $250=
=3D
=3D20
for a full =3DC2=3DBC of the kiln plus $35 (average) for the cost of high =
qual=3D
ity,=3D20
well seasoned, mixed cordwood (oak, cherry, and walnut). We generally us=
=3D
e=3D20
about =3DC2=3DBE of a cord and the average price of a cord is from $165 - =
$200=3D
.=3D20
Each firing will have 3 participants and I will take 1/4 of the kiln=3D20
myself so that I have a vested interest in the results. One participant m=
=3D
ust be=3D20
able to go into the kiln to help load. I will offer hands on instruction=
=3D
=3D20
for firing a wood kiln for those of you who may be new to the process. =3D=
20
Everyone must take part in the loading, firing, unloading, and cleaning up=
=3D
=3DE2=3D80=3DA6=3DE2=3D80=3DA6
.or at least a good portion of it. =3D20
I am happy to share Phil Rogers=3DE2=3D80=3D99 and my glaze formulas with =
any=3D20
participant and can make some suggestions about which ones work out the be=
=3D
st in this =3D20
kiln. He gave me his full glaze notes when he was here doing a workshop=
=3D
=3D20
last summer. I can furnish glazes for an additional cost of $20/person=3D=
20
(including me) and I will need someone to screen and wash three gallons of=
=3D
wood=3D20
ash. I will give instructions on how to do this and will supply all=3D20
needed/simple equipment to get this job done.=3D20
I have a firing coming up on September 14-15 (load one day and fire the =
=3D
=3D20
next). The May, June, and July firings filled within days.=3D20
Two spots filled within hours of my first notice yesterday and only one=3D=
20
opening is left for the September firing. We now need someone who is able=
=3D
to=3D20
go into the kiln to help set the rear tiers of shelves. =3D20
A deposit of $100 will hold your spot.=3D20
Make out a check to =3DE2=3D80=3D9CMonocacy River Pottery=3DE2=3D80=3D9D a=
nd mail it =3D
to:=3D20
Bruce Bowers=3D20
9219 Woodland Drive=3D20
Silver Spring, MD 20910=3D20
301-646-3481 (cell)=3D20
The next firing will be on July 21 and 22 with glazing on July 10 for=3D20
those of you enrolled in this group.=3D20
Each of you would need enough pots to cover a template 24" x 48" with a=3D=
20
height not to exceed 8 1/2" and you can include a couple of 12" pots for t=
=3D
he=3D20
top tier. Special provisions can be made for 18" pots, keeping in mind=3D=
20
that these will take up the space that two normal shelves would take up an=
=3D
d=3D20
will affect your total allotted space. Narrow forms give you the most ban=
=3D
g=3D20
for your buck.=3D20
Also, stacking and wadding one pot on top of another (only on unglazed=3D2=
0
surfaces) is a great space saver. I can show you how to do this even with=
=3D
=3D20
glazes by using wax resist as a decorative element. I just did a firing i=
=3D
n=3D20
which I fired 13 cup and saucer sets and 6 additional mugs and it took abo=
=3D
ut=3D20
one shelf (1/4 of your template). I always stack low bowls, plates,=3D20
serving trays, etc. and have learned to pack a lot of pots in a small spac=
=3D
e. I=3D20
can show you how to do the same.=3D20
Please bring your template to the firing so that we can move from person=
=3D
=3D20
to person as we load and, that way, make sure that there is good dispersio=
=3D
n=3D20
of work throughout the setting.=3D20
Please contact me ASAP if you are interested. Most cone 10 glazes will=3D=
20
work in wood firing. Clay bodies may be a bit more "iffy" and I will share=
=3D
my=3D20
observations over the years. All materials, including clays and glaze =3D=
20
materials (if you mix your own) are available at Clayworks Supply in =3D20
Baltimore.=3D20
Phoenix, Loafers Glory, Standard 508, and Standard 410 are good options,=
=3D
=3D20
with Phoenix being a good bet since it is a medium colored body.=3D20
Please contact me by email or call 301-646-3481 with questions.=3D20
Best,=3D20
Bruce Bowers, _www.bowerswoodfireandpics.com_=3D20
(http://www.bowerswoodfireandpics.com/)