Claudia MacPhee on fri 13 apr 12


There is one at the school I work at. The controller is very simple to w=
ork. Yesterday I fired it for the 330th time. Mostly 06, but some cone 6 fi=
rings. Same elements. Changed the thermocouple three times and the switches=
once. Usually put a long hold at 200 F. The times for firing are within mi=
nutes of the first one. Tech support at SPS is very good. Their kiln guy is=
helpful and pleasant!

Claudia MacPhee Tagish, Yukon