anyone have gun metal cone 6?

updated thu 23 feb 12

 

Snail Scott on tue 21 feb 12


On Feb 21, 2012, at 2:33 PM, Daniel Hunter wrote:
> I'm looking for a gun metal dark gray or black...


Any of the various high-manganese 'bronze' or 'gold'
glaze recipes will be reliably gunmetal grey if applied
thinly or even not-quite-thickly.

-Snail

Daniel Hunter on tue 21 feb 12


I'm looking for a gun metal dark gray or black...does
anyone have a recipe they like?