u.p. woodfired kiln 4th.firing finishing the front setting

updated sun 5 feb 12

 

gary navarre on sat 4 feb 12


It look likes the weather is cooperating for a firing so=3D

Hey Folks,=3D0A=3D0A=3DA0It look likes the weather is cooperating for a fir=
ing so=3D
I'm glad I did all this work earlier even though it was well below freezin=
=3D
g the last few weeks. In real time I lit the Pignose yesterday and I'm lett=
=3D
ing the charge of mixed hard and soft wood cook down to nothing in 6-8 hour=
=3D
s just to do some drying of the wadding and any moisture in the greenware w=
=3D
hich was at or below 20% from house drying. Zach is going to help me pick u=
=3D
p some Elm sticks from a standing dead Peter cut down and I might cut some =
=3D
more Hemlock limbs just to add a little extra to the fuel pile. I'm not in =
=3D
any real hurry so I'll probably keep a small fire going and get useta worki=
=3D
ng hard again because I got a little soft staying in the house all winter. =
=3D
Thanks for watching and stay in there eh.=3D0A=3D0Ahttp://www.youtube.com/w=
atch=3D
?v=3D3D7Nzqk-JP9-E=3D0A=3DA0=3D0AGary Navarre=3D0ANavarre Pottery=3D0ANavar=
re Enterpris=3D
es=3D0ANorway, Michigan, USA=3D0Ahttp://www.NavarrePottery.etsy.com=3D0Ahtt=
p://ww=3D
w.youtube.com/GindaUP=3D0Ahttp://public.fotki.com/GindaUP/=3D0A