Hi Rimas,

I used items left over from the building of our house.
It's Flextile 52 Versatile Floor set mortar.
Then I used a sanded poly-grout from home Depot or Lowes.
I think I also used some left over water based poly granite sealer.

best regards
Gayle

--
Gayle Bair
Bainbridge Island WA
Tucson AZ
gayle@claybair.com
www.claybair.com


On Thu, Nov 17, 2011 at 3:46 AM, Rimas VisGirda wrote:

> Hi, what is the adhesive you used to attach your tiles to the backer boar=
d
> that has survived for ove 10 years? Thanks, -Rimas
>







--