spending the weekend in the clay studio

updated mon 7 nov 11

 

Deborah Thuman on sun 6 nov 11


I'm getting ready to do a glaze firing this coming Friday and
Saturday. This will be ^04 oxidation. The ^04 reduction wild hair has
been firmly and permanently removed. Hey, you gotta do stuff like that
sometimes.

Anyway, I've got photos of work that is about to be bisqued on my blog
if you'd like to see what I'm working on. I'm coil building bowls. The
best bowls are waiting to dry some more so I can apply underglaze. I
finally figured out what I was doing wrong - I was building out and up
rather than up and out. Or: oh, so that's what the rib is for.


Deb Thuman
http://debthumansblog.blogspot.com/
http://www.etsy.com/shop.php?user_id=3D5888059
http://www.facebook.com/pages/Deb-Thumans-Art-Page/167529715986