On Sat, Sep 10, 2011 at 1:49 PM, John Britt wro=
te:
With all this talk of revisions of glazes: I revised Pinnell Blue Celadon a=
t
cone 10
and put the recipe on the blog with an image:

It is nice. But don't tell anyone the recipe because you'll never get it
anyway!

(Use the capitalist handshake to get in ..





Though I may be kicked out of the Capitalist Club for revealing the secret,
here is a short instructional video on how to perform the handshake:
https://www.youtube.com/watch?v=3DJ0g27yEu-AU

Take care.

...James

James Freeman

"All I say is by way of discourse, and nothing by way of advice. I should
not speak so boldly if it were my due to be believed."
-Michel de Montaigne

http://www.jamesfreemanstudio.com
http://www.flickr.com/photos/jamesfreemanstudio/
http://www.jamesfreemanstudio.com/resources

John Britt on sat 10 sep 11


With all this talk of revisions of glazes: I revised Pinnell Blue Celadon=
=3D
at cone 10=3D20
and put the recipe on the blog with an image:

http://ncclayclub.blogspot.com/2011/09/blue-celadon-cone-10.html

It is nice. But don't tell anyone the recipe because you'll never get it =
=3D
anyway!
=3D20
(Use the capitalist handshake to get in ...or send the checks "it's worth=
=3D
it dot=3D20
com")=3D20=3D20

Owner, President, CEO, CFO and head janitor of the Glaze Free-Trade Socie=
=3D
ty=3D20
john britt pottery . com

James Freeman on sun 11 sep 11


On Sun, Sep 11, 2011 at 11:14 AM, John Britt wr=
ote:
James,

That's it. (The fact that you know and watch the Simpsons tells me a lot
about
you- sicko.)




Guilty as charged!

To be truthful, I don't watch TV per se, Simpsons or otherwise. Haven't in
a dozen years. We have no cable, no satellite, and no set new enough for
over the air reception. In violation of my neo-luddite roots, we do have a=
n
ancient television set hooked to a dvd machine, and I do typically treat
myself to a nightly episode of The Simpsons as I enjoy an ice-cold bottle o=
f
Founders Brewery "Dirty Bastard Ale", which was, of course, named after me.

All the best.

...James

James Freeman

"All I say is by way of discourse, and nothing by way of advice. I should
not speak so boldly if it were my due to be believed."
-Michel de Montaigne

http://www.jamesfreemanstudio.com
http://www.flickr.com/photos/jamesfreemanstudio/
http://www.jamesfreemanstudio.com/resources

Richard Burkett on mon 12 sep 11


Hi John,
The secret part is that you can deflocculate the glaze and solve the craw=
=3D
ling=3D20
problem. There's been a lot of talk about flocculating glazes, but someti=
=3D
me one=3D20
needs to go the other way with glazes high in plastic clay like Grolleg.

Richard

John Britt on mon 12 sep 11


Great idea, I will give it a try. I sometimes do it to spray glazes.

johnbrittpottery.com