additives for throwing water

updated thu 8 sep 11

 

Dan Saultman on tue 6 sep 11


"Am I the only person that puts teatree oil in my water for throwing to
keep it fresher longer? Does anyone else add anything to their throwing
water to make it smell more pleasant or stay bacteria free longer?"
DJ Brewer.

Dear DJ,
I add a couple drops of laundry chlorine bleach.
You don't need much. It makes yucky gray clay become white
immediately and smells clean.
Give it a gentle stir.

Question: Does your tea oil make the water more slippery? That's what
I'm looking for.


Dan

Dan Saultman
Detroit
http://www.saultman.com