ravenscrag clear at cone 6=3d?windows-1256?q?=3dfe?=3d

updated fri 2 sep 11


Claudia MacPhee on thu 1 sep 11

I have used that base many times without problem. I use it without the f=
rit, just straight on in my wood kiln. Never had any problems with it.
However, never put red wine in any of my pots either. Have you checked it f=
or crazing?? Did the wine dye the entire bottom or just craze lines?
You could contact the people at Plainsman Clays, they might be able to help=

Claudia MacPhee Tagish, Yukon