search  current discussion  categories  glazes - misc 

fw: glazecal

updated tue 9 aug 11

 

Edouard Bastarache on mon 8 aug 11


Randall,

up here we live in metrics,
2,000 grams of dry raw materials give about 1 american gallon
of liquid glaze after water is added.
So, like you we get 5 gallons using 10,000 grams of dry
raw materials.
For glaze testing we use 200 grams.

"Vive le Metrique"


Gis,

Edouard Bastarache Spertesperantisto=3D20
Sorel-Tracy

Quebec


http://www.flickr.com/photos/30058682@N00/
http://edouardbastarache.blogspot.com/
http://edouardbastaracheblogs2.blogspot.com/
http://www.facebook.com/edouard.bastarache
http://blogsalbertbastarache.blogspot.com/






--=3D20
Randall in Atlanta
http://wrandallmoody.com