So my ^1 reduction firing went real good .... I'll post pics later on. The
clay body is Cumming's ^1 for throwing has the fired look of Yixing
ware....seems completely vitrified, rings clear as a bell. Kind of excited
about this. ( also it used almost no propane, compared to ^6)

-- Eric