Dinah Snipes Steveni on fri 3 jun 11


Hi Jenny and List

I used to use that body in the UK and the David Leach porcelain. We bisqued=
to 1020d c and fired to 1253 d c with an hour soak at top. Yeah, high but=
no tell-tale damp spots on the Young Chang! :) I think 1260 would be cons=
idered ^9 by most folks; into ^10 by the time the heat work completed. Wha=
t are your Orton cones telling you?


Dinah
Mount Vernon, WA.
www.dinahsnipessteveni.com