platters coming up

updated mon 19 jan 98

 

John Tilton on sun 18 jan 98

As far as platter edges coming up during drying, I have found that if I
fire the clay to maturity they will settle back down in the fire. Clay
memory.

I have however painted the edge and the first 3 inches towards the
middle of the inside of the platter, and that helps them stay flat.

John Tilton
Alachua, FL