teal glaze possibility ^6 ox

updated sun 6 mar 11

 

Dinah Snipes Steveni on sat 5 mar 11


This is for May Luk who was asking a couple of days ago. I downloaded this =
from John Post's website/recipes about a year ago. I've not tested it.

Ferro F 3134 20.9
Feldspar - Custer 26.2
Wollanstonite 20
Kaolin - EPK 15.6
Silica 17.3

+ 10% Mason Stain #6268
+ 3% Rutile


Dinah
Dianthus Ceramics
Mount Vernon, WA.