Randall Moody on fri 4 mar 11


I am starting to use Lazertran decals in my work and was wondering if anyon=
e
has any recommendations. I am firing the work to ^6, applying the decals an=
d
then firing to ^08 but I have heard that it is good to fire the decals to
one cone lower than the glaze firing. I don't want all of the details to
disappear. The paper is pricey so I would rather not have to waste too many
sheets.
Thanks in advance!

--
Randall in Atlanta
http://wrandallmoody.com