Yes, you can rehydrate dried out glazes.

Cautions: Make sure to let the glaze sit overnight or longer to =3D
rehydrate well. If you sieve too soon it is a big mess of lumps and =3D
clumps.

If you have too much water do NOT pour it off. All glazes contain some =3D
water soluble matter,you do not want to get rid of it. If the glaze =3D
turns out too thin, let it air dry on its own.

Lili Krakowski
Be of good courage