I found a cone 6 oxidation fake ash glaze on June Perry's Shambhala Pottery
site. I really like this glaze. I normally add copper oxide or cobalt for
different shades of blue or green. I would like to make a red gold glaze
with darker drips. Can you tell me what to add to this glaze to get the
color I want?

Fake ash glaze
46 Ferro Frit 3195

34 Whiting (calcium carb)

20 EPK

Thanks,
Judy Smith