Cathi Newlin on sat 20 nov 10


I was pretty pleased with the results of my latest firing (for a change...)
Tested 3 glazes, and while not a one turned out as I expected, I got
some fun results nonetheless.

All my ware survived, and I'm really happy with the lot.
Still, as always, I'd welcome any input on the glaze results...
http://squarepegarts.blogspot.com/2010/11/nov-19-firing-and-glaze-tests.htm=
l

Hope everyone's having a great weekend!
--
Cathi Newlin, Angels Camp, Ca
box49@caltel.com
http://www.cnewlin.com

William & Susan Schran User on sun 21 nov 10


On 11/20/10 5:20 PM, "Cathi Newlin" wrote:

> All my ware survived, and I'm really happy with the lot.
> Still, as always, I'd welcome any input on the glaze results...
> http://squarepegarts.blogspot.com/2010/11/nov-19-firing-and-glaze-tests.h=
tml

Looked at your test of the temmoku, recipe has 10% iron, so it should be
black/brown no matter oxidation/reduction. Did you forget to add the iron?
Does your test batch look iron red?

Bill

--