Just to clarify where on my kiln I'm asking about corbeling I took 6 new s=
hots and added then to the bottom of the ongoing album ...

http://public.fotki.com/GindaUP/ca/kpap/uphwfkl3/ (scroll down)

The captions explain some of my ideas of where to set the bricks. If we lo=
ok through the demolition photos we can see the different degrees of heat d=
istribution through the bricks. The top part of the firebox doesn't actuall=
y get as hot as one might think, if all the heat is being drawn into the ch=
amber with a good draft.