Liz Gowen 1 on sun 31 oct 10


Judy I know the Cuzaks fire cone 10 reduction. The blue you are looking at
on her piece looks a lot like one of hers I have and she said it was a
mystery bucket from another potter .You know the kind where you made an
oops and when it is gone oh well. Best to try another persons work. You
should be able to get decent blues in ^6 but I don't have one that is like
this. Liz Gowen

Subject: What is this medium blue speckled glaze?

I keep seeing pictures of pottery with this blue glaze that I love, but I
can not find a recipe for it. It seems to be a popular glaze because I hav=
e
seen it used by lots of pottersThe saucer was made by Mary Cuzack. Here is
the URL http://ww2.nscc.edu/smith_judy/blue.htm

thanks,
Judy Smith