slaking glazes aka steeping

updated tue 12 oct 10

 

Dinah Snipes Steveni on mon 11 oct 10


Yes. Leave raw materials to slake for 24 hours and sieve a couple of times =
to thoroughly disperse materials. They'll be thoroughly wetted AND you can =
siphon off top water to arrive at proper consistency for spraying/dipping/p=
ainting.


Dinah