Lee Brozgol on sat 2 oct 10


After bisque firing, my ware is covered with a chalky residue. So are the=
=3D
shelves=3D20
in my Skutt electrical kiln. I am using a low fire white earthenware cla=
=3D
y fired to=3D20
Cone 04. What causes this residue? Can it be prevented; and, if so, how=
=3D
?=3D20=3D20

Thanks!