mel jacobson on thu 16 sep 10


i was able to get a decent replica of the orange color
that was on about half of the pots fired yesterday.

it is a cloudy day, and i shot this in the shade with my nikon.
it is almost perfect in color in the photo.
clayart page/click below..third picture.

this orange color has peeked at us before, but never full
pots like this. iron bearing body, bone ash temmoku under.
it is hard to believe this is all 10% or more iron in all three glazes.
mel (just interesting.)